MAIN APPLICATIONS OF THIS PRODUCT ARE IN THE:
Road construction – production of bituminous concrete
- In the bituminous concrete (fundament compounds) – It replaces 50-70% of weight index of the crushed stone (about 86%), sand (about 10%) and bitumen (about 4%)
High rise construction
- Production of concrete compounds, it replaces 50-70% in weight index the crushed stone
TECHNICAL PARAMETERS OF THE “Gg”
- Density – 2200-2800 kg/m3
- Compression strength – 800-1200 MPa
- Tensile strength – 35 – 85 MPa
- Module of elasticity – 47 000 – 100 000 MPa
- Hardness (Moos) – 5 – 7
- Specific heat capacity in room temperature: 0.63 – 1.05 W/(kg.K)
Heat conduction of “Gg” at 100°С – 0.4-0.82 W/(m.K)